System upgrade reminder, Homepage update.
Stainless steel 301

Metal

Stainless steel 301

1.4310 | X10CrNi18-8

ProcessCNC Machining

Need this material for your project?

Upload your drawing and get manufacturing support from our engineering team.

Get Instant Quote

* Property values are for reference and may vary by alloy, temper, and processing conditions.

Stainless steel grade 301 possesses an exceptionally high work-hardening capacity, enabling enhanced strength and hardness through cold working. It simultaneously exhibits outstanding elasticity, toughness and impact resistance, making it an ideal choice for manufacturing high-strength structural components and resilient parts.

Material Properties

Mechanical Properties

  • Yield strength

    205 - 515 MPa (Annealed)

  • Tensile strength

    515 - 760 MPa (Annealed)

  • Elongation

    40 - 60 %

  • Hardness

    156 - 165 HB

  • Young's modulus

    189 - 197 GPa

Thermal properties

  • Maximum operating temperature

    870 - 925 °C

  • Thermal conductivity

    14 - 16 W/(m·K)

  • Coefficient of thermal expansion

    16.5 - 17.5 μm/(m·℃)

Physical Properties

  • Density

    7.93 g/cm³

Electrical properties

  • Electrical resistivity

    65 - 77 μΩ·cm

Manufacturability

  • Manufacturability-Corrosion resistance

    Good

  • Manufacturability-Weldability

    Good